Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Grupo Repol Dinalon® A1S25 G35PV0 35% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Grupo Repol
Trade Name Dinalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Grupo Repol Dinalon® A1S25 G35PV0 35% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 160 MPa
23200 psi
ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 527
Flexural Strength 250 MPa
36300 psi
ISO 178
Flexural Modulus 8.00 GPa
1160 ksi
ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched >= 1.00 J/cm²

@Temperature 23.0 °C
>= 4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75/A
Vicat Softening Point >= 230 °C
>= 446 °F
50 N; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Glow Wire Test 960 °C
1760 °F
IEC 695