Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Grupo Repol Dinalon® A1S25 G35 35% Glass Fiber Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Grupo Repol
Trade Name Dinalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Grupo Repol Dinalon® A1S25 G35 35% Glass Fiber Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Flexural Strength 290 MPa
42100 psi
ISO 178
Flexural Modulus 9.50 GPa
1380 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75/A
Vicat Softening Point >= 230 °C
>= 446 °F
50 N; ISO 306
Users viewing this material also viewed the following: