Greene Tweed Xyfluor® 870 Fluorinated Elastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name Xyfluor®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Xyfluor® 870 Fluorinated Elastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Xyfluor® 870, a highly fluorinated elastomer compound, provides excellent chemical compatibility over a wide range of temperatures from -76°F to 450°F (-60°C to 232°C). Recommended for applications demanding a combination of low-temperature properties and chemical resistance, Xyfluor 870 reduces overall cost, as compared to standard fluoroelastomers, PTFE, and graphite, by extending equipment service life.Xyfluor 870 parts can be made through high-volume injection-molding processing. Additionally, prototype parts are available for product testingApplications:Xyfluor is ideal for use in demanding high-volume applications such as mechanical seals and gaskets in a range of metering pumps, valves and other high-performance equipment.Information provided by Greene Tweed.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 7.58 MPa
1100 psi
ASTM D1414
Tensile Strength, Yield 3.79 MPa
550 psi
@100% Elongation; ASTM D1414
Elongation at Break 160 %
160 %
ASTM D1414
Compression Set 20 %
20 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Descriptive Properties Value Comments
Color Black