Greene Tweed Xyfluor® 860 Fluorinated Elastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name Xyfluor®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Xyfluor® 860 Fluorinated Elastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Xyfluor® 860, a highly fluorinated elastomer compound, offers excellent chemical compatibility over a wide range of temperatures from -76°F to 450°F (-60°C to 232°C). Recommended for applications requiring a combination of low-temperature properties and chemical resistance, Xyfluor’s capabilities surpass those of standard fluoroelastomers, PTFE, and graphite. Additionally, Xyfluor reduces overall cost by extending equipment service life.Applications:Xyfluor works well in demanding applications such as mechanical seals, gaskets and other custom components in a variety of metering pumps, valves and other high-performance equipment.Information provided by Greene Tweed.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D1414
Tensile Strength, Yield 2.41 MPa
350 psi
@100% Elongation; ASTM D1414
Elongation at Break 250 %
250 %
ASTM D1414
Compression Set 30 %
30 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Descriptive Properties Value Comments
Color Black