Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz® SD625, a black-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resistance and low extractables similar to PTFE. Not only is it FDA and USP Class VI compliant, but Chemraz SD625 also passes USP Physicochemical Testing, USP , and has been tested to USP elastomeric closures, USP , making it the most comprehensively tested perfluoroelastomer on the market. Critical applications and difficult seal replacement locations where maximizing MTBR (mean time between replacement) is paramount will benefit greatly from Chemraz SD 625.With is outstanding performance in high temperatures, Chemraz SD625 delivers excellent performance in hot water and steam and in CIP/SIP processes. Chemraz SD625 is also well suited for dynamic applicationsChemraz components are available for use as O-rings, gaskets, sanitary seals and many other custom shapes.Applications:Mechanical sealsValvesPumpsMixersFermentersBiomedical equipmentCouplingsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 22.1 MPa
3200 psi
ASTM D1414
Tensile Strength, Yield 4.48 MPa
650 psi
@50% Elongation; ASTM D1414
13.1 MPa
1900 psi
@100% Elongation; ASTM D1414
Elongation at Break 135 %
135 %
ASTM D1414
Compression Set 23 %
23 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Descriptive Properties Value Comments
Color Black