Greene Tweed CHEMRAZ® 534 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 534 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE. Chemraz designs last longer and seal better in harsh environments at a wider range of temperatures than any other elastomer on the market. Chemraz solves some of the most difficult sealing problems encountered in many industries while delivering outstanding in-use cost effectiveness through custom components.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.12 g/cc
2.12 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 10.1 MPa
1460 psi
ASTM D1414
Tensile Strength, Yield 2.07 MPa
300 psi
@50% Elongation; ASTM D1414
4.69 MPa
680 psi
@100% Elongation; ASTM D1414
Elongation at Break 190 %
190 %
ASTM D1414
Compression Set 25 %
25 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color White