Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

GrafTech GRAFOIL® GHJ Non-Standard Internal Combustion Grade GHJ Laminate, Metal Reinforced

Category Carbon , Graphite
Manufacturer GrafTech International
Trade Name GRAFOIL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GrafTech GRAFOIL® GHJ Non-Standard Internal Combustion Grade GHJ Laminate, Metal Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GRAFOIL® Grade GHJ is a laminate made with GRAFOIL® Grade GTC flexible graphite mechanically attached to a perforated, low-carbon steel core. Its applications include: exhaust manifold gaskets, exhaust sealing, gasoline/diesel head gaskets, EGR valve sealing, and turbo charger gaskets. It can be certified to meet Ford material spec ESEM8 G201-A. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced. Laminate Construction: GRAFOIL® Grade GTC 0.0066" thick (prior to tanging) - Low-Carbon Steel Grade 1008 or 1010 (130 tangs per square inch) - GRAFOIL® Grade GTC
Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
Thickness 1170 microns
46.1 mil
Standard; Laminate
1420 microns
55.9 mil
Standard; Laminate
1680 microns
66.1 mil
Standard; Laminate
Mechanical Properties Metric English Comments
Compression Set 80 %
80 %
Air Aging (22 hours at 535°C)
80 %

@Pressure 34.5 MPa
80 %

@Pressure 5000 psi
after 5000 psi load
Descriptive Properties Value Comments
Compressibility (%) 26
at 5000 psi load
30
Air Aging (22 hours at 535°C)
Copyright © lookpolymers.com All Rights Reserved