Gouda Vuurvast SiC 90 Dense Refractory Brick

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast SiC 90 Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Very good thermal shock resistance, abrasion resistance as well as very good heat conductivity makes this SiC based brick very well suited for muffles as well as for applications under highly abrasive conditions.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.50 g/cc
0.0903 lb/in³
Apparent
Porosity 18 %
18 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 100 MPa
14500 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 8.50 W/m-K

@Temperature 1100 °C
59.0 BTU-in/hr-ft²-°F

@Temperature 2010 °F
11.0 W/m-K

@Temperature 650 °C
76.3 BTU-in/hr-ft²-°F

@Temperature 1200 °F
15.0 W/m-K

@Temperature 100 °C
104 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1700 °C
3090 °F
Deformation under load - t<sub>a</sub>
1700 °C
3090 °F
Component Elements Properties Metric English Comments
SiO2 92 %
92 %
Descriptive Properties Value Comments
Thermal Shock Resistance Min 30 cycles
DIN 51068