Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURON 170 Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 170 Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.60 - 2.70 g/cc
0.0939 - 0.0975 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 50.0 - 60.0 MPa

@Temperature 100 °C
7250 - 8700 psi

@Temperature 212 °F
Cold Crushing Strength
50.0 - 60.0 MPa

@Temperature 1300 °C
7250 - 8700 psi

@Temperature 2370 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.31 - 1.41 W/m-K

@Temperature 600 °C
9.09 - 9.79 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.35 - 1.45 W/m-K

@Temperature 100 °C
9.37 - 10.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.38 - 1.48 W/m-K

@Temperature 1300 °C
9.58 - 10.3 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1700 °C
3090 °F
Shrinkage -0.300 - 0.300 %

@Temperature 1300 °C
-0.300 - 0.300 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 85 %
85 %
Fe2O3 1.0 %
1.0 %
SiO2 6.0 %
6.0 %
Descriptive Properties Value Comments
ASTM Classification F
Material Consumption per 1 m3 2550 kg
Mixing Water 8-10 liters
per 100 kgs dry material