Gouda Vuurvast CURON 120 Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 120 Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 7.00 - 17.0 MPa

@Temperature 1000 °C
1020 - 2470 psi

@Temperature 1830 °F
Cold Crushing Strength
25.0 - 35.0 MPa

@Temperature 100 °C
3630 - 5080 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 100 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.510 - 0.610 W/m-K

@Temperature 600 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.550 - 0.650 W/m-K

@Temperature 1000 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Shrinkage -0.100 - 0.500 %

@Temperature 1000 °C
-0.100 - 0.500 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 33 %
33 %
SiO2 50 %
50 %
Descriptive Properties Value Comments
ASTM Classification A
Material Consumption per 1 m3 1900 kg
Mixing Water 13-16 liters
per 100 kgs dry material