Gouda Vuurvast B 1 Sp Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast B 1 Sp Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High mechanical strength and very low porosity are typical for this type of brick. Application: transition zone in cement kilns, incinerators, steel ladles.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.25 g/cc
0.0813 lb/in³
Apparent
Porosity 12 %
12 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.12 W/m-K

@Temperature 100 °C
7.77 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.25 W/m-K

@Temperature 650 °C
8.68 BTU-in/hr-ft²-°F

@Temperature 1200 °F
1.38 W/m-K

@Temperature 1100 °C
9.58 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1350 °C
2460 °F
1420 °C
2590 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 39 %
39 %
Fe2O3 <= 2.0 %
<= 2.0 %
SiO2 55 %
55 %
Descriptive Properties Value Comments
Segercone 33
Thermal Shock Resistance 10 cycles
DIN 51068
Copyright © lookpolymers.com All Rights Reserved