Gouda Vuurvast AK 55 S Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast AK 55 S Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This andalusite based brick is characterized by a low porosity and a good creep resistance (After 24 hours at 1350°C under a load of 0.2 MPa gives between 14th and 24th hour a creep of 0.006% per hour.) Application: anode baking furnaces, blast furnace stoves.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.45 g/cc
0.0885 lb/in³
Apparent
Porosity <= 15 %
<= 15 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 60.0 MPa
8700 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.61 W/m-K

@Temperature 100 °C
11.2 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.64 W/m-K

@Temperature 650 °C
11.4 BTU-in/hr-ft²-°F

@Temperature 1200 °F
1.72 W/m-K

@Temperature 1100 °C
11.9 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
1600 °C
2910 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 55 %
55 %
Fe2O3 <= 1.0 %
<= 1.0 %
Na2O or K2O <= 0.60 %
<= 0.60 %
SiO2 43 %
43 %
Descriptive Properties Value Comments
Segercone 36-37
Thermal Shock Resistance 30 cycles
DIN 51068