Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1440 °C
2620 °F
Component Elements Properties Metric English Comments
Aluminum, Al 10 %
10 %
Zirconium, Zr 90 %
90 %