Goodfellow Titanium 80/Chromium 20 Alloy

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Titanium 80/Chromium 20 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1560 °C
2840 °F
Component Elements Properties Metric English Comments
Chromium, Cr 20 %
20 %
Titanium, Ti 80 %
80 %