Goodfellow Nickel 81/Iron 19 Alloy

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Nickel 81/Iron 19 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1445 °C
2633 °F
Component Elements Properties Metric English Comments
Iron, Fe 19 %
19 %
Nickel, Ni 81 %
81 %