Goodfellow Manganese 70/Nickel 30 Alloy

Category Metal , Nonferrous Metal
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Manganese 70/Nickel 30 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1040 °C
1900 °F
Component Elements Properties Metric English Comments
Manganese, Mn 70 %
70 %
Nickel, Ni 30 %
30 %