Goodfellow Copper 56.4/Titanium 43.6 Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Titanium Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Copper 56.4/Titanium 43.6 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 980 °C
1800 °F
Component Elements Properties Metric English Comments
Copper, Cu 56.4 %
56.4 %
Titanium, Ti 43.6 %
43.6 %