Material Notes:
Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 6.29 g/cc
0.227 lb/in³
Component Elements Properties Metric English Comments
Aluminum, Al 20 %
20 %
Chromium, Cr 80 %
80 %