Goodfellow Carbon/Vinyl Ester Rod

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Vinyl Ester
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Carbon/Vinyl Ester Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Physical Properties Metric English Comments
Density 1.50 - 1.65 g/cc
0.0542 - 0.0596 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 900 - 1200 MPa
131000 - 174000 psi
Longitudinal
Elongation at Break 1.4 %
1.4 %
Longitudinal
Tensile Modulus 136 GPa
19700 ksi
Longitudinal
Flexural Strength 800 - 1000 MPa
116000 - 145000 psi
Longitudinal
Flexural Modulus 65.0 - 85.0 GPa
9430 - 12300 ksi
Longitudinal
Compressive Strength 900 - 1100 MPa
131000 - 160000 psi
Longitudinal
Descriptive Properties Value Comments
Volume Fraction Fibers, % 55-60