Material Notes:
Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 2.85 g/cc
0.103 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 610 MPa
88500 psi
Longitudinal
Tensile Strength, Yield 400 MPa
58000 psi
Elongation at Break 6.0 %
6.0 %
Tensile Modulus 100 GPa
14500 ksi
Component Elements Properties Metric English Comments
Aluminum, Al 77.9 %
77.9 %
Copper, Cu 3.3 %
3.3 %
Magnesium, Mg 1.2 %
1.2 %
Manganese, Mn 0.40 %
0.40 %
SiC 17.8 %
17.8 %
Descriptive Properties Value Comments
Volume Fraction SiC, % 17