Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global PP-100 General Purpose Polypropylene Homopolymer, Controlled Rheology

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global PP-100 General Purpose Polypropylene Homopolymer, Controlled Rheology.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 31.7 MPa
4600 psi
Type 1 Specimen, Rate: 2"/min; ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
Tangent; Rate 0.5"/min; ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
Unannealed; ASTM D648