Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global PC/ABS QX-7004 Molding Grade PC/ABS  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global PC/ABS QX-7004 Molding Grade PC/ABS  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 260 °C
10 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM D638
Tensile Modulus 2.28 GPa
331 ksi
ASTM D638
Flexural Yield Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 6.10 J/cm
11.4 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
Unannealed (0.250 in.); ASTM D648