Global N-3260 High Density Polyethylene, Yarn/Monofilament Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global N-3260 High Density Polyethylene, Yarn/Monofilament Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing nets, wire & cable insulators, auto parts, pipesInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638