Global MPP-140-C 40% Mica Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Mica Filler
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global MPP-140-C 40% Mica Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.9 MPa
5200 psi
ASTM D638
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
290 °F
ASTM D648