Global Atron 6601-B General Purpose Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Global Polymers Corporation
Trade Name Atron
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global Atron 6601-B General Purpose Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.13 - 1.15 g/cc
0.0408 - 0.0415 lb/in³
ASTM D792
Viscosity Measurement 45 - 55
45 - 55
Relative Viscosity
Mechanical Properties Metric English Comments
Tensile Strength, Yield 81.4 MPa
11800 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 119 MPa
17300 psi
ASTM D790
Flexural Modulus 3.09 GPa
448 ksi
ASTM D790
Izod Impact, Notched 0.571 J/cm
1.07 ft-lb/in
ASTM D256