Global 100-25 LDPE Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global 100-25 LDPE Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Commercial-grade, low-density polyethylene with good dimensional stability, toughness and softness.Good dimensional stabilitySoftGood toughnessApplications:CapsClosures
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50

@Thickness 3.17 mm
50

@Thickness 0.125 in
Durometer, Injection Molded; ASTM D2240
Tensile Strength at Break 56.5 MPa

@Thickness 3.17 mm
8200 psi

@Thickness 0.125 in
Injection Molded; ASTM D638
Tensile Strength, Yield 64.8 MPa

@Thickness 3.17 mm
9400 psi

@Thickness 0.125 in
Injection Molded; ASTM D638
Elongation at Yield 19 %

@Thickness 3.17 mm
19 %

@Thickness 0.125 in
Injection Molded; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 86.1 °C
187 °F
ASTM D1525
Descriptive Properties Value Comments
Forms Pellets
Processing Method Injection Molding