Glastic Laminates/Shapes TSF Fiberglass-Reinforced Polyester Laminate

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Glastic
Trade Name Laminates/Shapes
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic Laminates/Shapes TSF Fiberglass-Reinforced Polyester Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Glastic Corporation.NEMA GPO-1. General purpose, high impact, heat resistant, dimensionally stable, cold punching. Excellent hot compression.
Mechanical Properties Metric English Comments
Flexural Strength 154 MPa
22300 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
NEMA temperature
UL RTI, Electrical 130 °C
266 °F
UL RTI, Mechanical with Impact 130 °C
266 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Arc Resistance 127 sec
127 sec
ASTM D495