Gharda Chemicals Gafone™ T6300 Polysupersulfone (PSS)  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals Gafone™ T6300 Polysupersulfone (PSS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C Applications: Electrical Switches High Temperature Resistant Covers Electronic Applications Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Water Absorption 0.60 %
0.60 %
24 Hours; ASTM D570
Melt Flow 18.76 g/10 min

@Load 10.0 kg,
Temperature 380 °C
18.76 g/10 min

@Load 22.0 lb,
Temperature 716 °F
6`; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 92.0 MPa
13300 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Tensile Modulus 2.60 GPa
377 ksi
ASTM D638
Flexural Strength 121 MPa
17500 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ASTM D648
Glass Transition Temp, Tg 266 °C
511 °F
ASTM D3482
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL 94
Oxygen Index 40 %
40 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Dielectric Constant 3.1

@Frequency 50 Hz
3.1

@Frequency 50 Hz
ASTM D150
Dielectric Strength 12.4 kV/mm
315 kV/in
ASTM D149
Dissipation Factor 0.0040

@Frequency 50 Hz
0.0040

@Frequency 50 Hz
ASTM D150