Gharda Chemicals Gafone S 1320GF Polysulfone (PS)  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals Gafone S 1320GF Polysulfone (PS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Electrical & Electronic - Head lamp reflectors, Chip tray carriers, battery cases Industrial - Milking machine parts, Safety belts Medical - Surgical tools, Dialysis membranes Membrane applications Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Filler Content 20 %
20 %
Water Absorption 0.50 %
0.50 %
24 Hours; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Tensile Modulus 6.50 GPa
943 ksi
ASTM D638
Flexural Strength 148 MPa
21500 psi
ASTM D790
Flexural Modulus 6.50 GPa
943 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 165 °C
329 °F
Continuous Use; UL-746B
Deflection Temperature at 1.8 MPa (264 psi) 183 °C
361 °F
ASTM D648
Glass Transition Temp, Tg 187 °C
369 °F
ASTM D3482
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
Oxygen Index 35 %
35 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Dissipation Factor 0.0030

@Frequency 60 Hz
0.0030

@Frequency 60 Hz
ASTM D150
Arc Resistance 60 sec
60 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638