Material Notes:
Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical Resistance Good Surface Release properties Tg of 224°C Expected Continuous Temperature of 180°C Applications: Food Contact Medical Electrical and Electronics Auto Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Filler Content 15 %
15 %
Water Absorption 0.51 %
0.51 %
24 Hours; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 113 MPa
16400 psi
ASTM D638
Elongation at Break 3.4 %
3.4 %
ASTM D638
Tensile Modulus 5.70 GPa
827 ksi
ASTM D638
Flexural Strength 162 MPa
23500 psi
ASTM D790
Flexural Modulus 4.60 GPa
667 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ASTM D648
Glass Transition Temp, Tg 225 °C
437 °F
ASTM D3482
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL 94
Oxygen Index 39 %
39 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Dissipation Factor 0.010

@Frequency 1e+6 Hz
0.010

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 50 sec
50 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved