Material Notes:
More economical gasket where a PTFE envelope is not required.Raised, molded-in sealing rings seal with 75% less surface area for high performance in non-metallic flangesMedia: Water, very mild acids and causticsInformation provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 70
60 - 70
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C

@Pressure 1.72 MPa
300 °F

@Pressure 250 psi
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Color Off-White