Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock GYLON® 3530 PTFE Gasketing, Graphite Filler

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Garlock Rubber Technologies
Trade Name GYLON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock GYLON® 3530 PTFE Gasketing, Graphite Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE with graphite fillerGraphite-filled PTFE offers extremely low void content for minimal emissionsBlack GYLON® delivers long service against volatile hazardous pollutants (VHAP and VOC)Withstands high concentrations of hydrofluoric acids and other glass-dissolving mediaMedia: Monomer service, cryogenics, highly concentrated hydrofluoric acid, volatile hazardous air pollutants (VHAP)Information provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
estimated by MatWeb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C

@Pressure 8.27 MPa
500 °F

@Pressure 1200 psi
Continuous
Minimum Service Temperature, Air -268 °C
-450 °F
Electrical Properties Metric English Comments
Dielectric Strength <= 0.0787 kV/mm

@Thickness 1.59 mm
<= 2.00 kV/in

@Thickness 0.0625 in
Unconditioned; ASTM D149