Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock GRAPH-LOCK® 3128 HOCHDRUCK® Graphite Sheet Gasketing, Steel Reinforced

Category Carbon , Graphite , Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Garlock Rubber Technologies
Trade Name GRAPH-LOCK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock GRAPH-LOCK® 3128 HOCHDRUCK® Graphite Sheet Gasketing, Steel Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High performance multi-layer graphite with 316SS inserts provides high compressive strength, blow-out resistance, excellent handling properties and improved tightness.Pure exfoliated graphite flake material excels in extreme conditions, withstanding heat, pressure, and aggressive chemicalsProven fire-safeSeals easily under moderate bolt load, offers superior torque retentionRetains dimensional stability in high temperatures; seals tightly even during pressure fluctuationsInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Permeability 0.40
0.40
Gas Permeability, cc/min; DIN 3535 Part 4
Mechanical Properties Metric English Comments
Tensile Strength 31.0 MPa
4500 psi
ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 649 °C
1200 °F
Steam
454 °C

@Pressure 13.8 MPa
850 °F

@Pressure 2000 psi
Minimum Service Temperature, Air -240 °C
-400 °F
Component Elements Properties Metric English Comments
Carbon, C 99.85 %
99.85 %
Descriptive Properties Value Comments
Compressibility, % 30-40
ASTM F36
Creep Relaxation, % 10
ASTM F38
Sealability ASTM F37B, ml/hr 0.1
Nitrogen
0.2
ASTM Fuel A
Copyright © lookpolymers.com All Rights Reserved