Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock 98206 EPDM Sheet Rubber Gasketing

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 98206 EPDM Sheet Rubber Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ethylene propylene diene monomer (EPDM)Certified to NSF/ANSI 61.Information provided by Garlock Rubber Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C

@Pressure 1.21 MPa
275 °F

@Pressure 175 psi
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: