Garlock 8798 Neoprene Rubber Diaphragm, Nylon Insert

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 8798 Neoprene Rubber Diaphragm, Nylon Insert.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neoprene rubber with 13oz. nylon fabric insertCombines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any service conditionInformation provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 75
65 - 75
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Electrical Properties Metric English Comments
Dielectric Strength 5.04 kV/mm

@Thickness 3.17 mm
128 kV/in

@Thickness 0.125 in
Unconditioned; ASTM D149
Descriptive Properties Value Comments
Color Black