Garlock 7164 SBR Rubber Lining

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 7164 SBR Rubber Lining.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SBR rubber lining for protection applications such as chute lining and skirtboards.An optional duck fabric backing is available.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Tensile Strength >= 13.8 MPa
>= 2000 psi
16.5 MPa
2400 psi
Typical
Elongation at Break >= 300 %
>= 300 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F