Material Notes:
Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #362 is a white nitrile sheet made from FDA-approved ingredients per Z1 CFR 177.2600. It also meets "3A Sanitary Standards for Multiple-Use Rubber and Rubber-Like Materials used as product contact surfaces in dairy equipment," Number 18-01, Class III and IV. It has good resistance to oily and greasy food products and abrasion. This sheet is non-marking.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Tensile Strength >= 10.3 MPa
>= 1500 psi
11.7 MPa
1700 psi
Typical
Elongation at Break >= 400 %
>= 400 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F