Garlock 2940 Compressed Aramid Fiber Gasketing, SBR Binder

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 2940 Compressed Aramid Fiber Gasketing, SBR Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aramid fibers with a Styrene-Butadiene (SBR) Binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasoline.Information provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0608 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 10.3 MPa
1500 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 371 °C
700 °F
204 °C

@Pressure 6.89 MPa
400 °F

@Pressure 1000 psi
Continuous
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Color Grey-Black
Compressibility, % 7-17
ASTM F36
Creep Relaxation, % 23
ASTM F38
Sealability ASTM F37B, ml/hr 1
ASTM Fuel A
2
Nitrogen