Material Notes:
Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0608 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 10.3 MPa
1500 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 371 °C
700 °F
204 °C

@Pressure 6.89 MPa
400 °F

@Pressure 1000 psi
Continuous
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 10.0 kV/mm

@Temperature 121 °C,
Time 10800 sec
254 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
>= 13.5 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 342 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
1.02 kV/mm

@Thickness 1.59 mm
26.0 kV/in

@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
1.10 kV/mm

@Thickness 3.17 mm
28.0 kV/in

@Thickness 0.125 in
100% RH for 96 hours; ASTM D149
Descriptive Properties Value Comments
Color Black
Compressibility, % 7-17
ASTM F36
Creep Relaxation, % 25
ASTM F38
Sealability ASTM F37B, ml/hr 0.25
ASTM Fuel A
1
Nitrogen