Garlock 2564 C.I. NBR/CR/SBR Sheet Rubber, Polyester Insert

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 2564 C.I. NBR/CR/SBR Sheet Rubber, Polyester Insert.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2264 is a smooth finish NBR/CR/SBR sheet, constructed with polyester. For moderate oil resistant applications.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Tensile Strength >= 6.89 MPa
>= 1000 psi
8.27 MPa
1200 psi
Typical
Elongation at Break >= 300 %
>= 300 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F