Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

GRECO ISOPAK 540 ABS Resin

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer GRECO
Trade Name ISOPAK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOPAK 540 ABS Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame Retardant GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Melt Flow 3.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 42.7 MPa
6190 psi
ASTM D638
Flexural Yield Strength 68.6 MPa
9960 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Izod Impact, Notched 2.16 J/cm
4.04 ft-lb/in
ASTM D256 A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Flammability, UL94 V-0
V-0