GEHR Plastics POM-ESD Acetal, Antistatic

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer GEHR Plastics Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GEHR Plastics POM-ESD Acetal, Antistatic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear because of the high strength and smooth surface. There is a very low risk of stress cracks. POM-C exhibits a high thermal stability and a high resistance to chemicals. Improved electrical conductivity.Properties:no microporosityhigh strengthhigh rigidityhigh thermal stabilitylow water absorptionhigh dimension stabilitygood electrical insulating propertiesvery good sliding propertieshigh resistance to stress cracksnot resistant to high concentrated acidsdifficult to glue and paintApplications include bearings, fittings, gear wheels, parts for pumps, screws, bobbins, parts for textile industry, and medium for coating lines.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break >= 20 %
>= 20 %
ISO 527
Modulus of Elasticity 1.65 GPa
239 ksi
ISO 527
Flexural Strength 45.0 MPa
6530 psi
3.5%; ISO 178
Coefficient of Friction 0.20
0.20
DIN 53375
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ISO 75
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1.00e+11 ohm
<= 1.00e+11 ohm
VDE 0303
Descriptive Properties Value Comments
Acid Resistance no
Aromatic Resistance yes
Bondability no
CKW Resistance limited
Color Ivory
Hydrocarbonate Resistance yes
Hydroxide Resistance yes
Ketone Resistance yes
Physiological indifference according no
Resistance Against Hot Water yes
UV Stabilization no