Material Notes:
Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be achieved only after conditioning, this material must be conditioned again after annealing. In addition, this conditioning occurs with a longer storage in air automatically.Properties:high impact strength and stiffnesshigh impact and notching impact strengthhigh heat deflection temperaturegood at dampeninggood glide and limp home charactersgood chemical stability against organic solvents and fuelssize alteration by humidity absorption must be considereddimension stability, electrical and mechanical properties may become affected by absorbing moisture or waterApplications include bearing parts, gear wheels, pump parts, sliding rails, castors, and fittings.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 1183
Water Absorption 9.5 %
9.5 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Yield 20 %
20 %
ISO 527
Modulus of Elasticity 1.00 GPa
145 ksi
ISO 527
Charpy Impact, Notched NB
NB
ISO 179
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+10 ohm-cm
>= 1.00e+10 ohm-cm
VDE 0303
Surface Resistivity per Square >= 1.00e+10 ohm
>= 1.00e+10 ohm
VDE 0303
Dielectric Constant 7.0

@Frequency 1.00e+6 Hz
7.0

@Frequency 1.00e+6 Hz
DIN 53483
Dielectric Loss Index 0.30

@Frequency 1.00e+6 Hz
0.30

@Frequency 1.00e+6 Hz
DIN 53483
Descriptive Properties Value Comments
Aromatic Resistance limited
Color Natural
Hydrocarbonate Resistance limited
Ketone Resistance limited
Resistance Against Hot Water limited