Freudenberg Simrit V175 Aflasâ„¢ (TFE/P)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Freudenberg Simrit
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit V175 Aflasâ„¢ (TFE/P).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent resistance to acids, bases, water and amines. Widely used in oil fields. Avoid polar solvents and aromatic fuels. Compression set performance may be too high for some applications. Typically used as a coater/developer, resists stripping, CMP and cleaning
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Tensile Strength, Ultimate 13.7 MPa
1990 psi
Elongation at Break 240 %
240 %
Compression Set 18 %

@Temperature 200 °C,
Time 252000 sec
18 %

@Temperature 392 °F,
Time 70.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -10.0 °C
14.0 °F
Descriptive Properties Value Comments
Color Black