Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Freudenberg Simrit V115 Standard Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Freudenberg Simrit
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit V115 Standard Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar solvents, amines, anhydrous ammonia, skydrol, hydrazine and hot acids.
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Tensile Strength, Ultimate 15.0 MPa
2180 psi
Elongation at Break 185 %
185 %
Compression Set 10 %

@Temperature 200 °C,
Time 252000 sec
10 %

@Temperature 392 °F,
Time 70.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved