Freudenberg Simrit Simriz® 489 Ultra Pure FFKT Perfluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Freudenberg Simrit
Trade Name Simriz®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit Simriz® 489 Ultra Pure FFKT Perfluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of elasticity. Simriz® perfluoro elastomers close the material gap between inelastic PTFE and elastomers, which have poor temperature and chemical resistance properties. With a fluoridation level of 72%, FFKM elastomers have a level of resistance close to that of pure PTFE at 76%. At the same time, FFKM materials are so elastic that they are excellently suited to both static and dynamic seals. Simrit offers ISC O-Rings which are specifically optimised with respect to flexibility at low temperatures, resistance to high temperatures, hardness, tensile strength, elongation, compression set, or color.Information provided by Freudenburg-NOK.
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
Tensile Strength, Ultimate 13.5 MPa
1960 psi
Elongation at Break 235 %
235 %
Compression Set 20 %

@Temperature 250 °C
20 %

@Temperature 482 °F
70 hr
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air 0.000 °C
32.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Manufacturer specifies transparent but does not quantify