Material Notes:
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasoline and solvents; poor resistance to alkalis and acids.
Mechanical Properties Metric English Comments
Hardness, Shore A 41
41
Original Properties; ASTM D2240
40

@Temperature 100 °C
40

@Temperature 212 °F
Water Immersion, 70 hours; ASTM D2240
46

@Temperature 225 °C
46

@Temperature 437 °F
Air Aging, 70 hours; ASTM D2240
Tensile Strength, Ultimate 7.00 MPa
1020 psi
Original Properties; ASTM D412 Die C
5.95 MPa

@Temperature 225 °C
863 psi

@Temperature 437 °F
Air Aging, 70 hours; ASTM D412 Die C
Elongation at Break 532 %
532 %
Original Properties; ASTM D412 Die C
420.28 %

@Temperature 225 °C
420.28 %

@Temperature 437 °F
Air Aging, 70 hours; ASTM D412 Die C
Tear Strength 16.4 kN/m
93.6 pli
ASTM D624 Die B
Compression Set 20 %

@Temperature 175 °C,
Time 79200 sec
20 %

@Temperature 347 °F,
Time 22.0 hour
Plied Discs (B37); ASTM D395
Descriptive Properties Value Comments
Color Red
Low Temperature Brittleness Pass, no cracks
ASTM D2137
Volume Change (%), ASTM D471 2
Water Immersion for 70 hours at 100°C