Formosa Plastics Formolene® L62608A Film (Hexene Grade) LLDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® L62608A Film (Hexene Grade) LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexene Copolymer (High Antiblock)Applications: Heavy duty shipping sacksHeavy duty shipping sacksInformation provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
Melt Flow 0.80 g/10 min
0.80 g/10 min
ASTM D1238