Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® HP4000 Pipe HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® HP4000 Pipe HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density Hexene Copolymer Formolene® HP4000 is a high performance copolymer that is designed for the most demanding requirements of non pressure pipe applications. It has good long-term hoop strength performance, very high melt strength, and outstanding toughness even at low temperatures. Formolene® HP4000 meets all requirements of ASTM D4976 – PE 235. Formolene® HP4000 meets the requirements of ASTM F 2160 for use in solid wall HDPE conduit based pipe.Applications: Telecommunications Conduit and Non-Pressure Pipe ApplicationsInformation provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Condition A, B, C, F<sub>50</sub>; ASTM D1693
Melt Flow 0.16 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.16 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.5 MPa
5000 psi
2" (50mm) per min, Type IV; ASTM D638
Tensile Strength, Yield 22.1 MPa
3200 psi
2" (50mm) per min, Type IV; ASTM D638
Elongation at Break >= 500 %
>= 500 %
2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 0.758 GPa
110 ksi
ASTM D3350
0.965 GPa
140 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -90.0 °C
<= -130 °F
ASTM D746