Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® E900 Pipe HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® E900 Pipe HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E900 is a high molecular weight high density polyethylene (HMW-HDPE) resin designed for non-pressure pipe applications. Formolene® E900 is well balanced in overall physical properties and provides good stiffness for extrusion applications.Applications: Corrugated Pipe and Non-Pressure Pipe Extrusion ApplicationsInformation provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 400 hour

@Strain 15.0 %
400 hour

@Strain 15.0 %
ESCR by NCLS; ASTM F2136
ESCR 10% Igepal® >= 500 hour
>= 500 hour
Condition B; ASTM D1693
Melt Flow 0.040 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.040 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
High Load Melt Index 8.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
8.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
2" (50mm) per min; ASTM D638
Elongation at Yield >= 600 %
>= 600 %
2" (50mm) per min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved